| Major Characteristics |
Application |
High gloss and high flow Low blush property and antistatic High impact strength Good stiffness
|
General electric home appliance
|
| Properties |
Test Method |
Unit |
J-370A |
| Melt Flow Rate (MFR) 230º C |
ASTM D-1238 |
g/10min |
35.0 |
| Mold Shrinkage |
HPC Method |
% |
1.40 |
| Density2 |
ASTM D-1505 |
g/cm³ |
0.9 |
| Tensile Strength at Yield |
ASTM D-638 |
Kg/cm² |
280 |
| Ultimate Elongation |
ASTM D-638 |
% |
>100 |
| Flexural Modulus of Elasticity |
ASTM D-790 |
Kg/cm² |
16,000 |
| Hardness(Rockwell) |
ASTM D-785 |
R |
95 |
| IZOD Impact Strength (23º C) |
ASTM D-256 |
Kg*cm/cm |
8.0 |
| IZOD Imp.Strength (-10º C) |
ASTM D-256 |
Kg*cm/cm |
3.5 |
| DuPont Imp.Strength(-10º C) |
HPC Method |
|
45 |
| Heat Resistance (130º C) |
Air Oven |
Hour |
>500 |
| Heat Distortion Temperature |
ASTM D-648 |
º C |
125 |
| Flammability |
UL |
- |
HB |
| Above data are not the spec of products, but only for reference |
|