| Major Characteristics |
Application |
High gloss Low blush property High stiffness & Good impact strength(FM)
|
General electric home appliance
|
| Properties |
Test Method |
Unit |
JH-370B |
| Melt Flow Rate (MFR) 230º C |
ASTM D-1238 |
g/10min |
27.0 |
| Mold Shrinkage |
HPC Method |
% |
1.40 |
| Density2 |
ASTM D-1505 |
g/cm³ |
0.90 |
| Tensile Strength at Yield |
ASTM D-638 |
Kg/cm² |
220 |
| Ultimate Elongation |
ASTM D-638 |
% |
>100 |
| Flexural Modulus of Elasticity |
ASTM D-790 |
Kg/cm² |
12,000 |
| Hardness(Rockwell) |
ASTM D-785 |
R |
85 |
| IZOD Impact Strength (23º C) |
ASTM D-256 |
Kg*cm/cm |
11.0 |
| IZOD Imp.Strength (-10º C) |
ASTM D-256 |
Kg*cm/cm |
6.0 |
| DuPont Imp.Strength(-10º C) |
HPC Method |
|
>100 |
| Heat Resistance (130º C) |
Air Oven |
Hour |
>500 |
| Heat Distortion Temperature |
ASTM D-648 |
º C |
100 |